Use a hair dryer not a heat gun. Much more forgiving. Inside out of wind. Heat slowly and press out with a gloved hand. Slowly work it out from edges to center. The plastic wants to go back to the set of the original shape. Once shape is returned you may be able to buff it with a scotch brite pad to restore the texture. Watch some YouTube videos on this first for starters.